Electrolytic reduction of alumina to aluminium by the Hall-Heroult process is carried out in the presence of:

  • A
    $NaCl$
  • B
    Fluorite
  • C
    Cryolite which forms a melt with lower melting temperature
  • D
    Cryolite which forms a melt with higher melting temperature

Explore More

Similar Questions

Low grade $Cu$ ores are available and $Zn$ and $Fe$ scraps are also available. Which scrap among the two would be more suitable for reducing the leached $Cu$ ore (economically)?

The slag formed during the extraction of $Fe$ is...........

Which of the following is not added during the extraction of silver by the cyanide process?

In which of the following isolations is no reducing agent required?

Which form of iron has the highest melting point?

Vedclass Products

For Students

Vedclass Test Series

Mock tests in real JEE/NEET style with performance analysis. 5-day free trial.

Start Free Trial
For Teachers

Exam Paper Generator

Generate Set A/B/C/D exam papers from 7.5L+ questions in 2 minutes. 3 chapters free.

Try Free
For Institutes

Online Exam Module

Live online exams with unlimited students, 360° analytics & white-label branding.

See Demo